  4. Enhanced functionalities of isovalently substituted 0.67(Bi1-xLaxFe0.97Ga0.03O3)-0.33(BaTiO3) relaxor piezoceramics synthesized via air quenching
 
  • Details

Enhanced functionalities of isovalently substituted 0.67(Bi1-xLaxFe0.97Ga0.03O3)-0.33(BaTiO3) relaxor piezoceramics synthesized via air quenching

Source
Journal of Solid State Chemistry
ISSN
00224596
Date Issued
2025-01-01
Author(s)
Paliwal, Srishti
Mondal, Prosun
Singh, Akhilesh Kumar
DOI
10.1016/j.jssc.2024.125049
Volume
341
Abstract
The isovalently substituted lead-free binary solid solution, 0.67(Bi<inf>1-x</inf>La<inf>x</inf>Fe<inf>0.97</inf>Ga<inf>0.03</inf>O<inf>3</inf>)-0.33(BaTiO<inf>3</inf>) (BF-BT) (x ≤ 0.07), has been synthesized by solid state ceramic method via air quenching sintering. FTIR and XRD along with Rietveld structure refinement confirmed a pure perovskite phase with a pseudocubic structure (space group Pm 3‾ m) for developed compositions. SEM revealed a dense microstructure with fine grain size (<1.5 μm) and minimal porosity. XPS analysis reveals predominantly Bi<sup>+3</sup> and Fe<sup>+3</sup> states, along with oxygen vacancies (V<inf>O</inf><sup>··</sup>). Ferroelectric studies demonstrated a maximum remanent polarization (Pr) of 12.3 μC/cm<sup>2</sup> and coercive field E<inf>C</inf> of 30.95 kV/cm for La<sup>3+</sup> concentration of x = 0.03. Overall decrement in Pr can be attributed to dipolar defect-induced random fields reducing the activation barrier for domain nucleation. Leakage current measurement reveals improved resistivity (∼10<sup>8</sup> Ω cm) up to an applied field of 30 kV/cm. Dielectric measurements unveiled two frequency-dependent anomalies in temperature dependence above room temperature, indicative of diffuse phase transitions. The Vogel-Fulcher model depicted an increasing freezing temperature (from 465 K for x = 0.01–551 K for x = 0.07) and decreasing activation energy (from ∼0.61 eV to 0.07 eV) with increasing La<sup>3+</sup> concentration. The estimated diffuseness parameter around ∼2 suggested relaxor behavior. Doping with La resulted in increased dielectric permittivity at 10 kHz (from 4100 to 24066), showcasing the efficacy of site engineering in augmenting the functional properties of BF-BT for high-temperature dielectric and transducer applications.
Unpaywall
URI
https://d8.irins.org/handle/IITG2025/28580
Subjects
Air quenching | BiFeO3–BaTiO3 | Ferroelectric | Lead-free | Piezoelectric
IITGN Knowledge Repository Developed and Managed by Library

Built with DSpace-CRIS software - Extension maintained and optimized by 4Science

  • Privacy policy
  • End User Agreement
  • Send Feedback
Repository logo COAR Notify