Repository logo
  • English
  • العربية
  • বাংলা
  • Català
  • Čeština
  • Deutsch
  • Ελληνικά
  • Español
  • Suomi
  • Français
  • Gàidhlig
  • हिंदी
  • Magyar
  • Italiano
  • Қазақ
  • Latviešu
  • Nederlands
  • Polski
  • Português
  • Português do Brasil
  • Srpski (lat)
  • Српски
  • Svenska
  • Türkçe
  • Yкраї́нська
  • Tiếng Việt
Log In
New user? Click here to register.Have you forgotten your password?
  1. Home
  2. Scholalry Output
  3. Publications
  4. A comparative analysis of InAs quantum dot heterostructure with equal and varying sub-capping layer thickness using digital alloy approach
 
  • Details

A comparative analysis of InAs quantum dot heterostructure with equal and varying sub-capping layer thickness using digital alloy approach

Source
Proceedings of SPIE the International Society for Optical Engineering
ISSN
0277786X
Date Issued
2022-01-01
Author(s)
Kumar, Ravindra
Kumar, Ajay
Saha, Jhuma  
Chakrabarti, Subhananda
DOI
10.1117/12.2633322
Volume
12200
Abstract
In current study, the variation of sub-capping thickness of InGaAs strain reducing layer (SRL) of InAs quantum dot heterostructure using digital alloy approach is presented. The thickness of 6 nm SRL of conventional structure (sample A) is divided equally with 2 nm thickness (sample B) by using digital alloy approach. Further, using such approach, this thick 6 nm capping is divided in unequal fashion for sample C (1 nm, 2 nm and 3 nm) and sample D (3 nm, 2 nm and 1 nm) from InAs QD towards top GaAs layer. The In-content inside the SRL of the sample A is 15%, whereas, In-content inside the divided-SRL is considered as 45%, 30% and 15% for all other samples. Such composition of SRLs helps in reducing the In-out diffusion, minimizing the lattice mismatch at InAs QD-SRL and SRL-top GaAs layer interfaces, and also reduces the strain inside the overall heterostructures. Two strains, namely hydrostatic and biaxial are calculated by using Nextnano for all the structures and compared simultaneously. The hydrostatic strain inside the QD of sample D is reduced by 4.74%, 1.07% and 2.269% and the biaxial strain inside the QD of sample D is improved by 1.66%, 0.696% and 1.276% as compared to that of samples A, B and C, respectively. The computed PL emission of samples A, B, C and D are observed to be 1305 nm, 1365 nm, 1349 nm and 1375 nm, respectively. Hence, sample D is the optimum choice for fabricating future opto-electronic devices.
Unpaywall
URI
https://d8.irins.org/handle/IITG2025/26285
Subjects
Digital Alloy Capping Layer | Equal and Unequal Sub Capping | InAs/InGaAs | Photoluminescence | Quantum Dots | Strain
IITGN Knowledge Repository Developed and Managed by Library

Built with DSpace-CRIS software - Extension maintained and optimized by 4Science

  • Privacy policy
  • End User Agreement
  • Send Feedback
Repository logo COAR Notify